Rymar Premium Wood Coating
Application Suggestions for Decks

  1. Let new wood dry for 30 days.
    After project completions, allow wood to dry (cure) for 30 days before starting the sealing procedure.
  2. Clean
    To clean, first wet wood.  Then use Rymar Rinseable soap and follow the directions on the box.  Rinse, let dry, then seal.
  3. Sealing Your Project
    Apply coating until it no longer penetrates.  Brush out any puddles of coating that develop.  Let dry for at least 48 hours before using, longer drying time may be required in cooler, damper weather.  Coating may be applied with a brush, sprayer, or by dipping.  Premium  requires step 4.
    Xtreme is a wet on wet application.  Seal 3-4 boards, seal them again while wet or tacky; this equals 2 coats and won't require step 4.
  4. Resealing with Premium Coating
    After 90 days clean surface with Rymar Rinseable soap and water, rinse and let dry.  Apply coating, again being careful not to allow puddles of coating to develop.  Allow to dry before using deck.

Do Not apply coating when these conditions exist ...

  • Do Not apply coating if you have not read the warnings and instructions on label of container.
  • Do Not apply coating if the wood is wet.
  • Do Not apply coating if the wood is dirty.
  • Do Not apply coating if the air temperature is below 45 degrees or above 90 degrees.
  • Do Not apply coating if the surface temperature of the wood is above 90 degrees.

Do apply coating ...

  • Apply coating after it has been stirred well and also stir frequently during application.
  • Apply coating the entire length of 2 or 3 boards at a time for uniform color appearance.
  • Apply coating with a brush, sprayer or by dipping.
  • Apply coating only after checking the color of each can by brushing a small test area.
  • Clean equipment with mineral spirits and dispose of rags properly.